You can see where around corners and even some straight runs it is peeling up. I’m running first layer at an agonizing 15 mm/s. Using hatchbox pla filament, just dried in dehydrator. 200° nozzle and 70° bed. The glass is freshly cleaned with soap and water, I just did several atomic pulls, I’ve trammed at different heights using a feeler gauge, and absolutely nothing is working. Any one have any ideas?

You are viewing a single thread.
View all comments
6 points

Increase the temp on your first couple layers by 5°. I’ve found that really helps with adhesion. If you’re still having difficulty with certain prints try using a brim.

permalink
report
reply
2 points

This was the brim printing. But increasing temp did seem to help!

permalink
report
parent
reply

3D Printing

!3dprinting@lemmy.ml

Create post

For everyhting 3D printing related.

Please be excellent to each other :)

Icon by Freepik, Banner photo by Thiago Medeiros Araujo

Community stats

  • 231

    Monthly active users

  • 163

    Posts

  • 796

    Comments

Community moderators