Hi there,

I’m wondering if I could get some advice on why my prints are always failing at 0.2mm layer height

Attached is a pic, the first layers are perfect but as it gets to layer 3-4 I the print does not stick to the previous layers!

Printing at 0.1mm is absolutely perfect, first layer is perfect etc (in my opinion)

Just wanted to have the option for a 0.2mm height so the prints don’t take as long.

Printer is Kingroon KP3S Pro V2 with Klipper Slicer is OrcaSlicer

I can share configs from either if needed, or more close up pics.

Cheers

5 points
*

You may be heavily underextruding on your 0.2mm setting, if it works at 0.1mm. Since the printer depends on extruding the right amount of material to build up to the nozzle tip, if you underextrude it won’t build up high enough, and that 4th or 5th layer won’t be close enough to the nozzle for the new plastic to be pressed down into it and stick.

Bump up those extrusion rates, slow down the movement feedrates, and make sure your nozzle and extruder motor are all clean and not slipping.

permalink
report
reply
3 points

That’s a good point - I remember calibrating the extrusion multiplier for 0.1mm but not for 0.2mm, never thought that larger layer sizes would need independent calibrations!

permalink
report
parent
reply
2 points

Yeah, extruder scaling is not perfectly linear, as you scale it faster the plastic slips more on the drive rolls, the heat input increase means the melt rate will not be perfect, and you have to fight the viscosity of liquid plastic.

permalink
report
parent
reply
1 point

Brilliant, thanks for the insight! Hopefully orcaslicer has a multiplier for each layer height - not just per filament

permalink
report
parent
reply
3 points

Would bumping up your printing temp do anything?

permalink
report
reply
2 points

It’s already running 225 for PLA since it’s a hardened steel nozzle, but I tried it on 230 with the same result

permalink
report
parent
reply
2 points

Is your filament dry? Less than 40% humidity? This happened to me with humid filament

permalink
report
reply
2 points

Ah really! It could be possible it’s too moist - It’s been out a month or so. I’ll have to invest in a filament dryer. Appreciate the reply

permalink
report
parent
reply
6 points

No need to get a purpose built dryer actually. Your heated bed will actually do exactly what you need. Flip a plastic container upside down over the bed with your filament underneath, set the bed to ~50-60C for PLA, and let it go for a couple hours.

permalink
report
parent
reply
2 points

Great idea thanks! 😀

permalink
report
parent
reply

3DPrinting

!3dprinting@lemmy.world

Create post

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

  • No bigotry - including racism, sexism, ableism, homophobia, transphobia, or xenophobia. Code of Conduct.

  • Be respectful, especially when disagreeing. Everyone should feel welcome here.

  • No porn (NSFW prints are acceptable but must be marked NSFW)

  • No Ads / Spamming / Guerrilla Marketing

  • Do not create links to reddit

  • If you see an issue please flag it

  • No guns

  • No injury gore posts

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

Community stats

  • 2K

    Monthly active users

  • 1.3K

    Posts

  • 17K

    Comments